Cracks in concrete and foundations: what to look for, and who decides
As at · 13 sources
Ultimate Foundations ·
The short answer
Concrete shrinks as it cures, and some cracking comes with that: the joints cut into a slab decide where the cracks go, not whether they happen. Other cracks come from the ground moving under a house, the steel inside the concrete rusting, or loads the concrete was not designed for. Which kind a crack in your house is, and whether it matters, is for a structural engineer who has seen the house.
Key points
- MBIE's guidance for Canterbury houses says concrete shrinks as it cures and gains strength. Good mix design, correctly placed reinforcing, adequate curing and correctly positioned shrinkage control joints will not eliminate the cracking, but they keep the cracks to a minimum and confine them to acceptable locations.1
- MBIE's guidance sets out indicator criteria for foundation damage and says they are not absolutes: they are indicators only, a full assessment of the damage is required to decide whether to repair or rebuild, and where it is unclear whether a criterion applies to a particular situation, professional engineering input should be sought. It says repairs may be needed even inside its limits.2
- The Natural Hazards Commission says that with a concrete slab there are fewer things you can do yourself to check its condition, stability and strength. It says not to go under the house if you think the foundations have weakened or are unstable, or if there may be a risk to your safety, and that if something does not look right when you check your foundations, you should talk to a licensed building professional before doing any work yourself.3
What causes cracks in concrete?
Many things, and a crack on its own does not say which. Some cracks form before the concrete has hardened. Others come later, as it dries, warms and cools, or as something works on it from outside.
BRANZ says cracks that form before concrete hardens come from plastic shrinkage, where the concrete dries too quickly before its final set, especially in floor slabs, or from plastic settlement, where reinforcing, embedded items or formwork restrict its movement as it is placed and compacted. Cracks after it hardens generally come from restrained drying shrinkage, differential moisture movement, thermal expansion and contraction, corrosion products building up on the steel, freeze-thaw cycles, alkali-aggregate reaction or sulphate attack (chemical cracking, which may indicate significant durability problems that were already there), and overloading, creep or loads beyond the design loads (structural cracking).4Do new concrete slabs crack?
They can, and a slab is built expecting it. Joints are cut or formed in a new slab so that the cracks from shrinkage open along lines chosen in advance, rather than wherever the concrete pulls apart. The joints do not stop the cracking.
MBIE's guidance says shrinkage control joints are cut to a quarter of the slab's thickness, generally within 24 hours of the pour, or a crack former is cast in the bottom of the slab. They do not stop cracking: they make the cracks form along lines set in advance. Random cracks can still form if the cutting is delayed, the mix was too wet, or the curing was wrong.5MBIE's guide to tolerances in new houses puts it this way, as a statement about slabs in general:
MBIE's guide to tolerances, materials and workmanship in new residential construction notes: “Some cracking in a concrete slab is common and is not necessarily a sign of poor workmanship.”6Does the weather on the day change how a slab cracks?
It does, and the number people watch is usually the wrong one. What a fresh slab answers to is not how warm the afternoon got. It is how far the temperature falls between the pour and the next morning. Concrete moves as it cools, and the first night is when it has the least strength to resist that movement. A run of mild days with cold nights is harder on a new slab than a steady cool week, which is why the joints want to be in place before the first night rather than the next working day.
Canterbury gives that swing more room than most places. The gap between a day's high and its low is wider inland than it is on the coast, so the same forecast does not mean the same thing at Hanmer Springs as it does at Kaikōura. A mild afternoon inland can still be followed by a night cold enough to matter.
No Canterbury council sets a temperature below which a pour may not go ahead, requires frost protection, or changes when inspections are available in winter. There is no published threshold to look up. A single number would be a poor fit for a place where the overnight fall matters more than the daytime figure, and the decision sits with the people on site on the day.
If you go looking for a figure for your own town, be careful which town it is. The published climate summary for Canterbury does not have a weather station everywhere. Rolleston, Lincoln, Leeston and Kaiapoi are not among the places it reports, so a frost or snow figure quoted for any of them was recorded somewhere else and carried across.
What signs point to a problem with a foundation?
Cracks are one sign among several. The Natural Hazards Commission lists what to look for, inside the house and out:
The Natural Hazards Commission lists warning signs that can point to a possible issue with your foundations, and says to take photos of them. Inside: cracks or gaps in ceilings and walls; doors and windows that stick (older timber joinery can also swell or shrink with the seasons); a sloping or uneven floor, which could indicate that the foundations have moved; cracked or uneven ceramic tiles; and stretched or loose carpet or vinyl. Outside: walls that are cracked or crumbling; exposed piles that may be loose or damaged; and water damage, ponding, or soil that has moved, sunk or slumped away from the foundation.7A floor that feels out of level is measured, not judged by eye or by a door that sticks.
MBIE's guidance says sticking doors and windows and cracked or wrinkled wall linings may suggest the floor is no longer level, but shaking distortion can cause similar effects, and that the key check is taking levels on the floor surface, or on something close to it such as the tops of skirting boards.8MBIE also names one shape of crack in a foundation wall as an indicator:
MBIE's guidance says foundation cracks that widen with height are a good indicator of some differential settlement of the foundation, which may come from an earthquake or from long-term differential settlement on weak soils.9Who decides whether a crack is structural?
A structural engineer, looking at the whole house. MBIE's guidance for Canterbury houses does not judge a foundation by its cracks alone: it looks at how far the house has settled, how far the floor has stretched, and what has happened to each part of the foundation, together.
MBIE's guidance assesses damage to a house foundation from three things together: differential and overall settlement; how far the floor and foundations have stretched sideways; and damage to particular parts of the foundation. Significant settlement can mean a foundation rebuild even when damage to its parts is minor, and severe damage to particular parts can be repaired locally if settlement is minor.10Walls of unreinforced brick or block are singled out:
MBIE's guide for Canterbury builders on below-floor work says specific engineering advice is required to assess damage to unreinforced brick or block masonry walls.11 Engineering New Zealand says you need a geotechnical engineer to assess ground conditions and decide a suitable foundation design, and to design foundations and retaining walls, and a structural engineer to assess the safety of a structure such as a retaining wall. It links a search of the register of Chartered Professional Engineers, and says being a member of Engineering New Zealand does not mean an engineer is also a CPEng.12How bad is a horizontal crack in a foundation?
A structural engineer can tell you, by looking at the wall and at the house around it.
Can a crack let the steel inside the concrete rust?
It can. Water and air get into concrete through cracks, and the steel is what they reach.
BRANZ lists cracks that let gases and liquids into concrete among the things that speed up corrosion of the reinforcing steel, and says cracks that follow the line of a bar can cause severe corrosion problems even if the crack is quite narrow.13What rusting steel does to concrete is set out in Spalling, rusting steel and “concrete cancer”.
Can I fix a crack myself?
Before doing any work yourself, the advice from the Natural Hazards Commission, in the key points above, is to talk to a licensed building professional.
Who to contact
- A geotechnical engineer
- What the ground under your section is, and what it will carry. They investigate it and write the report the foundation is designed from.
- The engineer who designs your foundation
- What goes under the house, and why. Thickness, steel, beams and the system itself are settled here.
- Your council
- Whether the work needs a building consent, what has to be shown, and when it is inspected.
- The Licensed Building Practitioners register
- Whether the person doing restricted building work holds a licence for it. It is a free public search and it takes a minute.
- Us
- What we would build, what it would cost, and what we would need from you before we could start.
If you are told something is not possible, it is always worth asking which of these decided it. The ground and the Code are fixed. A design and a programme sometimes are not.
What we do here
UF builds pod raft foundations for and TC2 sites, and engineered foundations for TC3 sites, using Firth RibRaft, Allied SuperSlab or MAXRaft depending on what the engineer's plans specify. If you are building, send the plans and the address.
Sources
To find a chartered professional engineer, use the register search from Engineering New Zealand. The Natural Hazards Commission sets out its warning signs in full on its page about home foundations.
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), Appendix A4.2. Checked . Read the source
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), section 2.3, Table 2.3 note and explanatory notes. Checked . Read the source
- Natural Hazards Commission Toka Tū Ake, Your home's foundations. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 6.4.3 and 6.4.5. Checked . Read the source
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), Appendix A4.2.1, Figure A4.1. Checked . Read the source
- MBIE, Guide to tolerances, materials and workmanship in new residential construction, 2015, section 2.2, Concrete floors. Checked . Read the sourceSource: Ministry of Business, Innovation and Employment, Guide to tolerances, materials and workmanship in new residential construction 2015. © Crown copyright 2015, licensed under CC BY 3.0; quoted or restated in part. Licence terms
- Natural Hazards Commission Toka Tū Ake, Your home's foundations. Checked . Read the source
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), sections 2.4 and 2.5. Checked . Read the source
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), Appendix A4.3.1. Checked . Read the source
- MBIE, Repairing and rebuilding houses affected by the Canterbury earthquakes, Part A, Version 3 (December 2012), section 2.2. Checked . Read the source
- MBIE, The guide for Canterbury builders, Below-floor work, April 2013, pages 6 and 7. Checked .
- Engineering New Zealand, Find an engineer. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 6.4.2 and 7.5.2 to 7.5.3. Checked . Read the source
Page history
Current as at .