Spalling, rusting steel and “concrete cancer”
As at · 12 sources
Ultimate Foundations ·
The short answer
Spalling is concrete breaking away at an edge or a surface. Rusting steel inside the concrete is one cause: the rust takes up more room than the steel it came from, and pushes off the concrete covering it. Whether a particular patch is serious is for a structural engineer or a concrete repair specialist who has seen it.
Key points
- BRANZ says corrosion of reinforcing steel is one of the most common and obvious causes of poor concrete durability in New Zealand, and that the first outward signs are usually small cracks in the concrete along the lines of the reinforcing and, sometimes, rust stains. Rust takes up three times the volume of the steel it forms from, so it makes the concrete covering the steel flake off or spall. Once the steel is exposed it corrodes faster, and its ability to resist tensile stress is reduced, which can lead to cracking or structural failure.1
- BRANZ says the most frequent and most severe cases of reinforcement corrosion in New Zealand can be attributed to chloride ions. It puts the greatest areas of risk within 100 m of the high tide mark, or within 500 m if downwind of a prevailing onshore wind, and lists chloride sources including salt spray, seawater, calcium chloride set accelerators, contaminated aggregates or sand, reinforcing or formwork coated with salt spray, and soil water high in chloride.2
- BRANZ says that when corrosion has already occurred, you should obtain specialist advice before undertaking repairs. It says repairs are easier and cheaper if done when damage is first noticed, and that unless concrete repairs are on a minor scale, they are a highly specialised task that should only be undertaken by specialists, depending on thorough investigation and diagnosis. Regular visual checks and tapping can pick up crack movement, spalling, efflorescence and rust staining.3
What is spalling?
Concrete breaking away at an edge or a surface. MBIE's definition is written for stone and masonry, and BRANZ uses the word for concrete:
MBIE's guide to tolerances in new houses defines a spall, citing NZMP 4212:1998, as a break at the edges of stone or other masonry materials, through weathering, chemical action or excess loading. BRANZ uses the word for the concrete covering the steel when corroding steel pushes it off.4Why does the steel inside concrete rust?
Steel inside good concrete is protected by the concrete around it. It starts to rust when that protection is lost, and there are two main ways that happens.
BRANZ says fresh concrete, with a pH of 12.5 to 13, forms a protective layer on the steel inside it. Corrosion starts when that changes: through carbonation, the concrete losing its alkalinity, or through chlorides beyond a critical level. How fast it goes depends on water and oxygen. Moist concrete corrodes faster than dry, the greatest danger is cyclic wetting and drying with marine salts, and corrosion of reinforcing steel in dry interior concrete is unlikely.5 BRANZ says carbonation is carbon dioxide from the air entering concrete, in the presence of moisture, and lowering its alkalinity. It generally happens faster around external corners and in poor-quality, permeable concrete, and whether the steel corrodes depends on how fast it moves in compared with the depth of concrete covering the steel. Adequate cover of well-compacted, low- permeability concrete increases the time until the concrete around the steel carbonates; in good- quality concrete, that can take many decades.6Chlorides, from salt, are the other, and BRANZ puts the greatest risk near the coast (see the key points). Other things speed rusting up as well:
BRANZ also lists impact or abrasion that removes the concrete covering the steel, contact between dissimilar metals, such as a copper pipe touching slab reinforcing, and acid or sulphate attack among the things that speed up corrosion.7Cracks are one of the ways in, and Cracks in concrete and foundations sets that out.
Is spalling a structural problem?
It can be. Where the spalling is in concrete that holds the house up, such as a foundation, a beam or a slab, show it to a structural engineer before anything is repaired.
Engineering New Zealand says you need a geotechnical engineer to assess ground conditions and decide a suitable foundation design, and to design foundations and retaining walls, and a structural engineer to assess the safety of a structure such as a retaining wall. It links a search of the register of Chartered Professional Engineers, and says being a member of Engineering New Zealand does not mean an engineer is also a CPEng.8What if a foundation is crumbling?
Show it to a structural engineer. What to look for around a foundation, inside the house and out, is in Cracks in concrete and foundations.
What else can break up a concrete surface?
Salt crystals forming just under the surface, and sodium sulphate attacking the cement paste. BRANZ also lists freezing and thawing among the causes of cracking once concrete has hardened.
The Cement & Concrete Association of New Zealand says salt crystals forming below the surface of concrete are not visible unless the crystal growth is enough to cause surface scaling, and that sodium sulphate can attack hydrated cement paste and cause surface scaling. On basement walls or slabs without a damp-proof membrane, it says, vapour-permeable surface treatments may make salts concentrate beneath the treated surface, leading to surface flaking or spalling. BRANZ lists freeze-thaw cycles as a cause of cracking after concrete hardens.9What is efflorescence on concrete?
A deposit, usually white, left on concrete or masonry by salts that water has carried to the surface. Usually it is a matter of looks. When it keeps coming back, it is a sign that water is still getting in.
BRANZ says efflorescence generally appears as a white deposit, sometimes brown, green or yellow, on masonry and concrete. It forms when soluble salts dissolve in moisture inside the wall, are carried to the surface, and stay there when the moisture evaporates. It does not affect the performance of blockwork, brickwork or concrete, but is considered unsightly, and it is common on new walls and will generally disappear naturally over time.10 BRANZ says efflorescence will recur if the wall has not completely dried or water has been absorbed, and that if it persists, it shows water is continuing to get into the masonry or concrete, perhaps through inadequate flashing or damp-proof course. Cleaning it does not cure the problem; it only removes the symptoms. BRANZ advises against washing it off with water or sandblasting it.11 The Cement & Concrete Association of New Zealand says efflorescence usually affects only the appearance of the concrete rather than its mechanical performance or durability. Occasionally, though, it may be a symptom of chemical reactions such as sulphate attack, and it may also indicate leaks in a water-retaining structure or an undesirable passage of water through other structures. Groundwater, it says, is a common source in basements, retaining walls and foundations.12How is spalling repaired?
The repair follows from finding out why the steel rusted, and the advice from BRANZ, in the key points above, is to get specialist advice before any repair is started.
Who to contact
- A geotechnical engineer
- What the ground under your section is, and what it will carry. They investigate it and write the report the foundation is designed from.
- The engineer who designs your foundation
- What goes under the house, and why. Thickness, steel, beams and the system itself are settled here.
- Your council
- Whether the work needs a building consent, what has to be shown, and when it is inspected.
- The Licensed Building Practitioners register
- Whether the person doing restricted building work holds a licence for it. It is a free public search and it takes a minute.
- Us
- What we would build, what it would cost, and what we would need from you before we could start.
If you are told something is not possible, it is always worth asking which of these decided it. The ground and the Code are fixed. A design and a programme sometimes are not.
What we do here
UF builds pod raft foundations for and TC2 sites, and engineered foundations for TC3 sites, using Firth RibRaft, Allied SuperSlab or MAXRaft depending on what the engineer's plans specify. If you are building, send the plans and the address.
Sources
To find a chartered professional engineer, use the register search from Engineering New Zealand.
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 1.0.1 and 1.0.3. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 1.0.2 and 6.2.1 to 6.2.5. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 1.0.5, 8.0.2 and 9.0.1 to 9.0.5. Checked . Read the source
- MBIE, Guide to tolerances, materials and workmanship in new residential construction, 2015, glossary; with BRANZ Bulletin 574, paragraph 1.0.3. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 3.0.1 to 3.0.2, 4.0.1 and 6.1.1 to 6.1.2. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 5.0.1, 5.2.1 and 6.1.3 to 6.1.4. Checked . Read the source
- BRANZ Bulletin 574, Preventing corrosion of reinforcing steel in concrete, August 2014, paragraphs 7.5.2 to 7.5.3. Checked . Read the source
- Engineering New Zealand, Find an engineer. Checked . Read the source
- Cement & Concrete Association of New Zealand, Information Bulletin IB 44, Efflorescence in Concrete, December 2004, Definitions, Significance and Surface Treatments; with BRANZ Bulletin 574, paragraph 6.4.5. Checked . Read the source
- BRANZ Bulletin 593, Efflorescence, February 2016, summary and paragraphs 1.0.1 to 1.0.3 and 2.0.1 to 2.0.2. Checked . Read the source
- BRANZ Bulletin 593, Efflorescence, February 2016, paragraphs 5.0.5 to 5.0.9. Checked . Read the source
- Cement & Concrete Association of New Zealand, Information Bulletin IB 44, Efflorescence in Concrete, December 2004, Definitions, Significance, Service Environment and Removal. Checked . Read the source
Page history